CORC  > 金属研究所  > 中国科学院金属研究所
Characterization of ferroniobium topologically close-packed phase inclusion in nickel-based 152 cladding of dissimilar metal welds
Li, Yifeng1,2; Wang, Jianqiu1; Han, En-Hou1
刊名JOURNAL OF NUCLEAR MATERIALS
2019-03-01
卷号515页码:267-275
关键词Topologically close-packed phase Dissimilar metal weld joint Welding inclusion Ferroniobium Microstructure characterization In-situ tensile
ISSN号0022-3115
DOI10.1016/j.jnucmat.2018.12.049
通讯作者Wang, Jianqiu(wangjianqiu@imr.ac.cn)
英文摘要Ferroniobium topologically close-packed (TCP) phase inclusions were found in the nickel-based152 nickel-based cladding of dissimilar metal weld joint in pressurized water nuclear reactor. A systematical investigation on the morphologies, microstructures and mechanical properties was conducted by using multi-scale techniques. The formation causes of the TCP-phase inclusion and its possible influences on crack initiation and propagation during long-term operation are also discussed. The ferroniobium TCP-phase inclusions originate from large-size ferroniobium supplement particles in 152 welding electrode flux during welding. The inclusion with core has a homogeneous kernel and a continuous transition zone between the core and eutectic zone, and the transition zone consists of columnar grain zone and isometric grain zone. The inclusion core is confirmed as single-phase rhombohedral Fe7Nb6 (mu phase), and columnar grain zone in the transition zone is also mainly Fe7Nb6, while the isometric grain zone and the Nb-rich phase in the eutectic zone are both mainly hexagonal Fe2Nb (Laves phase), the other phase in the eutectic zone is austenite. The Fe2Nb is formed by eutectic metallurgical reaction between inclusion core and 152 cladding. The average hardness of inclusion core (17.89 GPa) is over 4.5 times as high as cladding matrix (3.91 GPa). The TCP-phase inclusion is of higher cracking susceptibility than 152 cladding, and acts as the initiation of brittle cracks during in-situ tensile test. The ferroniobium TCP-phase inclusions are of higher cracking susceptibility than 152 cladding. (C) 2019 Elsevier B.V. All rights reserved.
资助项目National Key Research and Development Program of China[2016YFE0105200] ; Key Research Program of Frontier Sciences, Chinese Academy of Sciences[QYZDY-SSW-JSC012]
WOS研究方向Materials Science ; Nuclear Science & Technology
语种英语
出版者ELSEVIER SCIENCE BV
WOS记录号WOS:000456805800025
资助机构National Key Research and Development Program of China ; Key Research Program of Frontier Sciences, Chinese Academy of Sciences
内容类型期刊论文
源URL[http://ir.imr.ac.cn/handle/321006/131145]  
专题金属研究所_中国科学院金属研究所
通讯作者Wang, Jianqiu
作者单位1.Chinese Acad Sci, Inst Met Res, Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Liaoning, Peoples R China
2.Univ Sci & Technol China, Sch Mat Sci & Engn, Shenyang 110016, Liaoning, Peoples R China
推荐引用方式
GB/T 7714
Li, Yifeng,Wang, Jianqiu,Han, En-Hou. Characterization of ferroniobium topologically close-packed phase inclusion in nickel-based 152 cladding of dissimilar metal welds[J]. JOURNAL OF NUCLEAR MATERIALS,2019,515:267-275.
APA Li, Yifeng,Wang, Jianqiu,&Han, En-Hou.(2019).Characterization of ferroniobium topologically close-packed phase inclusion in nickel-based 152 cladding of dissimilar metal welds.JOURNAL OF NUCLEAR MATERIALS,515,267-275.
MLA Li, Yifeng,et al."Characterization of ferroniobium topologically close-packed phase inclusion in nickel-based 152 cladding of dissimilar metal welds".JOURNAL OF NUCLEAR MATERIALS 515(2019):267-275.
个性服务
查看访问统计
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。


©版权所有 ©2017 CSpace - Powered by CSpace