Coaxial anodic oxidation under dynamic electrolyte conditions for inner surface patterning of high-aspect-ratio and slim Ti tubes | |
Wang, Ye[1]; Sun, Lidong[1]; Xiang, Chengjie[1]; Zhao, Xiaoli[1]; Wu, Sujuan[1]; Zhang, Sam[2] | |
2017 | |
卷号 | 124页码:193-197 |
URL标识 | 查看原文 |
内容类型 | 期刊论文 |
URI标识 | http://www.corc.org.cn/handle/1471x/2975830 |
专题 | 重庆大学 |
推荐引用方式 GB/T 7714 | Wang, Ye[1],Sun, Lidong[1],Xiang, Chengjie[1],et al. Coaxial anodic oxidation under dynamic electrolyte conditions for inner surface patterning of high-aspect-ratio and slim Ti tubes[J],2017,124:193-197. |
APA | Wang, Ye[1],Sun, Lidong[1],Xiang, Chengjie[1],Zhao, Xiaoli[1],Wu, Sujuan[1],&Zhang, Sam[2].(2017).Coaxial anodic oxidation under dynamic electrolyte conditions for inner surface patterning of high-aspect-ratio and slim Ti tubes.,124,193-197. |
MLA | Wang, Ye[1],et al."Coaxial anodic oxidation under dynamic electrolyte conditions for inner surface patterning of high-aspect-ratio and slim Ti tubes".124(2017):193-197. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论