CORC  > 重庆大学
Varying the strong basal texture in a Mg-3Al-1Zn plate by a new wave-shaped interface rolling
Sun, Zheng[1]; Wu, Yang[2]; Xin, Yunchang[1]; Peng, Yanshuo[1]; Feng, Bo[1]; Liu, Qing[1]
2018
卷号213页码:151-153
URL标识查看原文
内容类型期刊论文
URI标识http://www.corc.org.cn/handle/1471x/2973563
专题重庆大学
推荐引用方式
GB/T 7714
Sun, Zheng[1],Wu, Yang[2],Xin, Yunchang[1],et al. Varying the strong basal texture in a Mg-3Al-1Zn plate by a new wave-shaped interface rolling[J],2018,213:151-153.
APA Sun, Zheng[1],Wu, Yang[2],Xin, Yunchang[1],Peng, Yanshuo[1],Feng, Bo[1],&Liu, Qing[1].(2018).Varying the strong basal texture in a Mg-3Al-1Zn plate by a new wave-shaped interface rolling.,213,151-153.
MLA Sun, Zheng[1],et al."Varying the strong basal texture in a Mg-3Al-1Zn plate by a new wave-shaped interface rolling".213(2018):151-153.
个性服务
查看访问统计
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。


©版权所有 ©2017 CSpace - Powered by CSpace