Hydrogen embrittlement of high strength steam turbine last stage blade steels: Comparison between PH17-4 steel and PH13-8Mo steel | |
Li, Xinfeng; Zhang, Jin; Fu, Qinqin; Akiyama, Eiji; Song, Xiaolong; Shen, Sicong; Li, Qizhen | |
刊名 | Materials Science and Engineering A |
2019 | |
卷号 | 742页码:353-363 |
关键词 | Cu-rich precipitates Hydrogen diffusion Hydrogen diffusion coefficients Hydrogen permeation Hydrogen solubility Last stage blades Precipitate strengthening Slow strain rate tensile test |
ISSN号 | 0921-5093 |
URL标识 | 查看原文 |
内容类型 | 期刊论文 |
URI标识 | http://www.corc.org.cn/handle/1471x/2828635 |
专题 | 西安交通大学 |
推荐引用方式 GB/T 7714 | Li, Xinfeng,Zhang, Jin,Fu, Qinqin,et al. Hydrogen embrittlement of high strength steam turbine last stage blade steels: Comparison between PH17-4 steel and PH13-8Mo steel[J]. Materials Science and Engineering A,2019,742:353-363. |
APA | Li, Xinfeng.,Zhang, Jin.,Fu, Qinqin.,Akiyama, Eiji.,Song, Xiaolong.,...&Li, Qizhen.(2019).Hydrogen embrittlement of high strength steam turbine last stage blade steels: Comparison between PH17-4 steel and PH13-8Mo steel.Materials Science and Engineering A,742,353-363. |
MLA | Li, Xinfeng,et al."Hydrogen embrittlement of high strength steam turbine last stage blade steels: Comparison between PH17-4 steel and PH13-8Mo steel".Materials Science and Engineering A 742(2019):353-363. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论