Influence of solidification conditions and alloying elements Re and Ti on micropores formed during homogenization of Ni base single crystal superalloy
Liu, JL; Meng, J; Yu, JJ; Zhou, YZ; Sun, XF; Liu, JL (reprint author), Chinese Acad Sci, Inst Met Res, Superalloy Div, Shenyang 110016, Liaoning, Peoples R China.
刊名JOURNAL OF ALLOYS AND COMPOUNDS
2018-05-25
卷号746页码:428-434
关键词High-temperature Creep X-ray Tomography Nickel Porosity Diffusion Growth Mechanisms Behavior Pores Model
ISSN号0925-8388
英文摘要The influence of withdraw rate during directional solidification and elements Re and Ti on the formation of micropores during homogenization in Ni base single crystal superalloy CMSX-4 is investigated by Xray tomography method. The results show that the number of micropores below 5 mm in sample solidified at 10 mm/min after homogenization at 1300 degrees C/3 h is greater than that in the case of 6 mm/min. The number of micropores below 10 mm in Re free and Ti free alloys is rather smaller than that of normal CMSX-4 alloy, while the number of micropores between 15 mm and 25 mm in Ti free alloy is relatively greater than that in Re free alloy. The variation of number of micropores is analyzed based on measurement of primary dendrite arm spacing (PDAS) and segregation ratios of alloying elements, the causes are mainly attributed to reverse segregation tendencies of Re and Ti and their remarkable diffusion coefficient difference, the increasing of PDAS also enhances the propensity of micropores formation during homogenization. (c) 2018 Elsevier B.V. All rights reserved.; The influence of withdraw rate during directional solidification and elements Re and Ti on the formation of micropores during homogenization in Ni base single crystal superalloy CMSX-4 is investigated by Xray tomography method. The results show that the number of micropores below 5 mm in sample solidified at 10 mm/min after homogenization at 1300 degrees C/3 h is greater than that in the case of 6 mm/min. The number of micropores below 10 mm in Re free and Ti free alloys is rather smaller than that of normal CMSX-4 alloy, while the number of micropores between 15 mm and 25 mm in Ti free alloy is relatively greater than that in Re free alloy. The variation of number of micropores is analyzed based on measurement of primary dendrite arm spacing (PDAS) and segregation ratios of alloying elements, the causes are mainly attributed to reverse segregation tendencies of Re and Ti and their remarkable diffusion coefficient difference, the increasing of PDAS also enhances the propensity of micropores formation during homogenization. (c) 2018 Elsevier B.V. All rights reserved.
学科主题Chemistry, Physical ; Materials Science, Multidisciplinary ; Metallurgy & Metallurgical Engineering
语种英语
资助机构National Natural Science Foundation of China [1671188, 51601192]
公开日期2018-06-05
内容类型期刊论文
源URL[http://ir.imr.ac.cn/handle/321006/79301]  
专题金属研究所_中国科学院金属研究所
通讯作者Liu, JL (reprint author), Chinese Acad Sci, Inst Met Res, Superalloy Div, Shenyang 110016, Liaoning, Peoples R China.
推荐引用方式
GB/T 7714
Liu, JL,Meng, J,Yu, JJ,et al. Influence of solidification conditions and alloying elements Re and Ti on micropores formed during homogenization of Ni base single crystal superalloy[J]. JOURNAL OF ALLOYS AND COMPOUNDS,2018,746:428-434.
APA Liu, JL,Meng, J,Yu, JJ,Zhou, YZ,Sun, XF,&Liu, JL .(2018).Influence of solidification conditions and alloying elements Re and Ti on micropores formed during homogenization of Ni base single crystal superalloy.JOURNAL OF ALLOYS AND COMPOUNDS,746,428-434.
MLA Liu, JL,et al."Influence of solidification conditions and alloying elements Re and Ti on micropores formed during homogenization of Ni base single crystal superalloy".JOURNAL OF ALLOYS AND COMPOUNDS 746(2018):428-434.