Kinetics of thermo-oxidative degradation of zinc borate/microcapsulated red phosphorus with magnesium hydroxide in flame retarded polypropylene composites. | |
Xiaolang Chen chenxl612@sina.com.cn; Jie Yu yujiegz@126.com; Zhu Luo; Shuchun Hu; Zuowan Zhou; Shaoyun Guo; Shengjun Lu | |
刊名 | Journal of Polymer Research
![]() |
2009 | |
卷号 | Vol.16 No.6页码:745-753 |
关键词 | Kinetics Magnesium hydroxide Polypropylene Red phosphorus Thermo-oxidative degradation Zinc borate |
ISSN号 | 1022-9760 |
URL标识 | 查看原文 |
内容类型 | 期刊论文 |
URI标识 | http://www.corc.org.cn/handle/1471x/1937615 |
专题 | 四川大学 |
作者单位 | 1.National Engineering Research Center for Compounding and Modification of Polymer Materials, Guiyang 550014, China. 2.Key Laboratory of Advanced Materials Technology Ministry of Education, School of Materials Science and Engineering, Southwest Jiaotong University, Chengdu 610031, China. 3.The State Key Laboratory of Polymer Materials Engineering, Polymer Research Institute of Sichuan University, Chengdu 610065, China. |
推荐引用方式 GB/T 7714 | Xiaolang Chen chenxl612@sina.com.cn,Jie Yu yujiegz@126.com,Zhu Luo,et al. Kinetics of thermo-oxidative degradation of zinc borate/microcapsulated red phosphorus with magnesium hydroxide in flame retarded polypropylene composites.[J]. Journal of Polymer Research,2009,Vol.16 No.6:745-753. |
APA | Xiaolang Chen chenxl612@sina.com.cn.,Jie Yu yujiegz@126.com.,Zhu Luo.,Shuchun Hu.,Zuowan Zhou.,...&Shengjun Lu.(2009).Kinetics of thermo-oxidative degradation of zinc borate/microcapsulated red phosphorus with magnesium hydroxide in flame retarded polypropylene composites..Journal of Polymer Research,Vol.16 No.6,745-753. |
MLA | Xiaolang Chen chenxl612@sina.com.cn,et al."Kinetics of thermo-oxidative degradation of zinc borate/microcapsulated red phosphorus with magnesium hydroxide in flame retarded polypropylene composites.".Journal of Polymer Research Vol.16 No.6(2009):745-753. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论